Table of Content
We are Popular Trader, Wholesaler of Lead Tin Bronze Manufacturer in India. It is used in Bushings for Electric Motor, Guide bushings for valves. Alloy High LTB Offers a Balance of Strength and Ductility to Obtain Desired Durability.
High Lead Tin Bronze Melting Point & Density
LTB Alloy Application

Heat Treatment of Tin Bronze
Conditions of Leded Bronze
Alloy High LTB Material Benefits
Lead Tin Bronze Advantages
Lead Tin Bronze Supplier in India View Characteristics
Dealer & Distributor of Leded Bronze Metal Packing & Delivered Areas

Alloy High LTB Material Disadvantages
Aluminum Bronze Steel Cutting Methods
Thermal Properties of High Lead Tin Bronze
| Thermal Properties | Metric | English |
|---|---|---|
| CTE, linear | 18.5 µm/m-°C Temperature 20.0 - 205 °C | 10.3 µin/in-°F Temperature 68.0 - 401 °F |
| Specific Heat Capacity | 0.376 J/g-°C | 0.0899 BTU/lb-°F |
| Thermal Conductivity | 52.0 W/m-K Temperature 20.0 °C | 361 BTU-in/hr-ft²-°F Temperature 68.0 °F |
| Melting Point | 855 - 945 °C | 1570 - 1730 °F |
| Solidus | 855 °C | 1570 °F |
| Liquidus | 945 °C | 1730 °F |
| Shrinkage | 1.1 % | 1.1 % |
Electrical Properties of Alloy High LTB Material
| Electrical Properties | Metric | English |
|---|---|---|
| Electrical Resistivity | 0.00001599 ohm-cm Temperature 20.0 °C | 0.00001599 ohm-cm Temperature 68.0 °F |
| Magnetic Permeability | 1.0 | 1.0 |
Equivalent Grade of Tin Bronze Metal
| Grade | UNS | SAE |
|---|---|---|
| North America | United States | |
| Bronze 85-5-5-5 Round Bar | 660 | C83600 |
| Bronze 83-7-7-3 Round Bar | 660 | C93200 |
Physical Properties of High Lead Tin Bronze
| Property | C90200 Tin Bronze | C90300 Tin Bronze |
|---|---|---|
Density |
0.318 lb/cu in. at 20 °C |
0.318 lb/cu in. at 20 °C |
Hardness, Brinell |
Brinell Hardness of 70 with a 500 kg |
Brinell Hardness of 70 with a 500 kg |
Tensile strength |
262 MPa |
310 MPa |
Specific Heat Capacity |
0.09 Btu/lb/°F at 20 °C |
0.09 Btu/lb/°F at 20 °C |
Thermal Conductivity |
36 Btu/sq ft/ft hr/°F at 20 °C |
43.2 Btu/sq ft/ft hr/°F at 20 °C |
Electrical conductivity |
13% IACS at 20 °C |
12% IACS at 20 °C |
Melting point solidus |
876 °C |
854 °C |
Melting point liquidus |
1046 °C |
1000 °C |
Tin Bronze Mechanical Properties
| Grade | Property | Hardness, Brinell | Tensile Strength, Ultimate | Tensile Strength, Yield | Elongation at Break |
|---|---|---|---|---|---|
| Bronze 83-7-7-3 Round Bar | Metric | 65 | 240 MPa | 125 MPa | 20 % |
| English | 65 | 34800 psi | 18100 psi | 20 % | |
| Bronze 85-5-5-5 Round Bar | Metric | 60 | 255 MPa | 117 MPa | 30 % |
| English | 60 | 37000 psi | 17000 psi | 30 % |
Leded Bronze Chemical Composition
| Grade | Al | Si | S | Fe | Sb | Pb | Ni | Zn | P |
|---|---|---|---|---|---|---|---|---|---|
| Bronze 85-5-5-5 Round Bar | - | 0.05 | 0.005 | 0.25 | 0.005 | 0.30 | 6.00 | - | 1.00 |
| Bronze 83-7-7-3 Round Bar | 0.005 | 0.005 | 0.08 | 0.20 | 0.35 | 0.30 | 1.00 | 4.0 | 8.0 |
Delivery Schedule of High Lead Tin Bronze Material
| Country | Country Name | Delivery Time |
|---|---|---|
| Singapore | 8 days | |
| Saudi Arabia | 7 days | |
| Egypt | 18 days | |
| South Africa | 25-30 days | |
| Jordan | 21 days | |
| Thailand | 7 days |
Copyright © 2024 Aashish Steel | All rights reserved. Design & SEO By MESOTEK